aluminum foil for hair salon

Aluminum foil for hairdressing

Parameters of aluminum foil for hairdressing Alloy: 8011 Temper: soft Type: roll Thickness: 9mic-30mic Length: 3m-300m Width: Custom Size Accepted Color: Customers' Request Treatment: Printed, Embossed Use: hair dressing Production: Hair Salon Foils, Hair Dressing Foil Main features and advantages of hairdressing foil: It is suitable for bleaching and dyeing h ...

foil plates aluminum

Aluminum foil for foil plate

Parameters Double bright side Alloy: 3003, 8011 etc Temper: O ( HO ), H22, H24 etc Thickness: 20 micron, 200 micron etc Width: 100mm, 600mm etc

1200 aluminum foil

1200 alloy aluminum foil

1200 aluminum foil details Alloy 1200 aluminum foil Temper F, O,H12,H16,H18,H22,H24,H26 Thickness 0.3-15mm Width*Length (10-1600mm)*C 1200 alloy aluminum foil parameters Chemical Composition of Alloy 1200 aluminium foil Si+Fe Cu Mn Zn Ti Mg Cr Other Al ≤1.0 ≤0.05 ≤0.05 ≤0.1 ≤0.05 - - 0.05(each) 0.15(total) 99.00 Mechanical propertiesof ...

industrial aluminum foil roll

Aluminum foil for industrial use

Parameters of industrial grade aluminum foil Alloy: 3003, 8011 etc Applications of industrial used aluminum foil Insulation, low temperature resistant, al pe laminited for packing, beverage industrial use and wine use etc

aluminum foil sticker

Aluminum foil for sticker

About us Henan Huawei Aluminum Co., Ltd. is the leader of many aluminum manufactures and suppliers in China. We strictly control the quality and focus on customers. We hope to have in-depth cooperation with you and provide you with high quality aluminum material products custom OEM services. If you want to get the newest and best prices by per kg or per ton standard weight, please contact us. Aluminum foi ...

The cause of pinhole in aluminum foil production process?

Aluminum foil pinhole has two main factors, one is the material, the other is the processing method. 1. Improper material and chemical composition will lead to a direct impact on the pinhole content of fake aluminum foil Fe and Si. Fe>2.5, Al and Fe intermetallic compounds tend to form coarse. Aluminum foil is prone to pinhole when calendering, Fe and Si will interact to form a firm compound. The number of ...

plain aluminum foil

The order of plain aluminum foil #05231048 ( export to UK )

Product name: plain aluminum foil SIZE (MM) ALLOY / TEMPER 0.1MM*1220MM*200M 8011 O

How to control the thickness difference of aluminum foil?

It is a characteristic of aluminum box rolling that the thickness deviation is difficult to control. The thickness difference of 3% is not difficult to control in the production of plate and strip, but it is more difficult to control in the production of aluminum foil. As the thickness of the aluminum box becomes thinner, its micro-conditions can affect it, such as temperature, oil film, and oil and gas concen ...

How is aluminum foil produced?

Cast-rolled aluminum foil production process Aluminum liquid, aluminum ingot -> Smelt -> Continuous roll casting -> Winding -> Cast roll finished product Plain foil production process Plain foil -> Cast-rolled coil -> Cold rolled -> Foil rolling -> Slitting -> Annealing -> Plain foil finished product The manufacture of aluminum foil is similar to making pasta at home. A large b ...

aluminum household foil 8011 in jumbo rolls

Delivery 20 tons aluminum household foil 8011 in jumbo rolls to Bosnia and Herzegovina

Household foil is widely used in cooking, freezing, preservation, baking and other industries. The disposable aluminum foil paper has the advantages of convenient use, safety, sanitation, no odor and no leakage. In the refrigerator or freezer, aluminum foil can be directly wrapped on the food, which can keep the food from deformation, avoid the water loss of fish, vegetables, fruits and dishes, and prevent the le ...

What is the cause of oil spots on aluminum foil?

The rolling oil and other oil stains remaining on the surface of the foil, which are formed on the foil surface to varying degrees after annealing, are called oil spots. The main reasons for oil spots: high degree of oil in aluminum foil rolling, or inappropriate distillation range of rolling oil; mechanical oil infiltration in aluminum foil rolling oil; improper annealing process; excessive oil on the surface ...